Abstract | Uniaxial hot compression tests were performed at constant temperature (T) and strain rate (ε ) in the ranges of 200-500 °C at an interval of 50 °C and 0.001-20 s. The flow stress data were used to develop the extrusion limit diagram for AZ31 and AM30 magnesium tubes. The extrusion limit diagram shows a wide region available for extruding AZ31 and AM30 seamless tubes, and comparison of the two extrusion limit diagrams shows that, the extrudability of AM30 alloy is better than that of AZ31 alloy. Actual extrusion trials validated the predicted temperature rise limit curve corresponding to the occurrence of surface cracking during the extrusion process. Magnesium tubes were successfully extruded according to the safe regions identified by the extrusion limit diagram. |
Keyword | AZ31 and AM30 magnesium alloys Extrusion limit diagram Magnesium seamless tubes |
URL | View the original |
Language | 英語English |
Fulltext Access | |
Document Type | Conference paper |
Collection | University of Macau |
Affiliation | 1.General Motors 2.Shanghai Jiao Tong University |
Recommended Citation GB/T 7714 | Wang Y.,Zeng X.,Ding W.,et al. Development and validation of extrusion limit diagram for AZ31 and AM30 magnesium alloys[C], 2007, 327-332. |
APA | Wang Y.., Zeng X.., Ding W.., Luo A.A.., & Sachdev A.K. (2007). Development and validation of extrusion limit diagram for AZ31 and AM30 magnesium alloys. Materials Science Forum, 546-549(PART 1), 327-332. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment